Abstract
In order to solve the problems such as the poor compatibility between the Ni-P-(SiC)p coating matrix metal bond and strengthening of the covalent bond, easy shedding of the enhanced particle and the deduction of the coating properties (SiC)p was surface-modified to (Ni/SiC)p by a simple electroless plating. Then (Ni/SiC)p particles were incorporated into the Ni-P plating solution to prepare Ni-P-(Ni/SiC)p electroless composite coatings. The experimental results show that; temperature, pH, stirring speed and adding amount of (Ni/SiC)p have great influence on the deposition amount and deposition rate of Ni-P-(Ni/SiC)p coating. The optimal experimental conditions are the temperature of 82-86°C, the pH range of 4.2-4.6, the stirring rate of 200 r/mim and the amount of particles of 10 g/L. SEM and EDS analyses show that Ni-P-(Ni/SiC)p coating is uniform and dense, the deposition of Ni, P and Si is large. Comparisons of the Ni-P coatings and the Ni-P-(SiC)p coatings by wear resistance experiment show that the Ni-P-(Ni/SiC)p coatings have good wear resisting properties. The (Ni/SiC)p achieved by surface modification can further improve the using performance of Ni-P-(SiC)p coatings.
| Original language | English |
|---|---|
| Pages (from-to) | 310-313+318 |
| Journal | Cailiao Kexue yu Gongyi/Material Science and Technology |
| Volume | 16 |
| Issue number | 3 |
| State | Published - Jun 2008 |
Keywords
- (Ni/SiC)
- Coatings
- Electroless plating
- Technical conditions
- Wear resistance
Fingerprint
Dive into the research topics of 'Technical conditions of Ni-P-(Ni/SiC)p coatings'. Together they form a unique fingerprint.Cite this
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver