Abstract

This paper summarises our recent cyclic nanoindentation experiment studies on a range of materials including single crystal and nanocrystalline copper, single crystal aluminium and bulk metallic glasses with different glass transition temperatures. The unloading and reloading processes of the nanoindentation curves have been analysed. The reverse plasticity will be discussed in the context of plastic deformation mechanisms involved. The effect of loading rates on the mechanical properties of materials upon cyclic loading will also be discussed.

Original languageEnglish
Title of host publicationMaterials Research Society Symposium Proceedings - Fundamentals of Nanoindentation and Nanotribology IV
Pages135-140
Number of pages6
StatePublished - 2008
Externally publishedYes
EventFundamentals of Nanoindentation and Nanotribology IV held at the 2007 MRS Fall Meeting - Boston, MA, United States
Duration: 26 Nov 200729 Nov 2007

Publication series

NameMaterials Research Society Symposium Proceedings
Volume1049
ISSN (Print)0272-9172

Conference

ConferenceFundamentals of Nanoindentation and Nanotribology IV held at the 2007 MRS Fall Meeting
Country/TerritoryUnited States
CityBoston, MA
Period26/11/0729/11/07

Fingerprint

Dive into the research topics of 'Reverse plasticity in nanoindentation'. Together they form a unique fingerprint.

Cite this