Preparation of expanded graphite with Fe3O4 nanoparticles

Research output: Chapter in Book/Report/Conference proceedingConference contributionpeer-review

Abstract

In this paper, it can be seen that the optimum mixture ratio of graphite to other contents (graphite: H2SO4: H2O2: HClO4) is 10(g):28(ml):1(ml):5(ml), which obtained the best expansion volume (191ml/g). The Fe3O4-expanded graphite composite material was prepared by FeCl3 solution of ethylene glycol with heating reaction in reactor. The graphite sheets within EG were nanoscales, four iron oxide nanoparticles were dispersed between holes of expanded graphite sheets. Evidently, the graphite nanosheets wrapped in the four iron oxide particles can be observed. It is clearly that the magnetic adsorption properties of particles are strength on EG/Fe3O4. In addition, the EG/Fe3O4 composite obtained by this process has a product (magnetite), which is proved of XRD characteristic peaks.

Original languageEnglish
Title of host publicationMaterials Design, Processing and Applications
Pages507-510
Number of pages4
DOIs
StatePublished - 2013
Externally publishedYes
Event4th International Conference on Manufacturing Science and Engineering, ICMSE 2013 - Dalian, China
Duration: 30 Mar 201331 Mar 2013

Publication series

NameAdvanced Materials Research
Volume690 693
ISSN (Print)1022-6680

Conference

Conference4th International Conference on Manufacturing Science and Engineering, ICMSE 2013
Country/TerritoryChina
CityDalian
Period30/03/1331/03/13

Keywords

  • Expanded graphite
  • Expansion volume
  • Four iron oxide nanoparticles

Fingerprint

Dive into the research topics of 'Preparation of expanded graphite with Fe3O4 nanoparticles'. Together they form a unique fingerprint.

Cite this