Abstract
Amorphous nano-sized silicoboron carbonitride (Si-B-C-N) powders with average grain size <50 nm were fabricated by high energy shaker mill using hexagonal boron nitride, graphite and amorphous silicon powders as starting materials. The powders were consolidated by spark plasma sintering at 1900° and 1950°C. Amorphous phase were partially retained in ceramic sintered at 1900°C. For ceramic sintered at 1950°C, amorphous Si-B-C-N ceramic transferred to hexagonal BN and cubic SiC.
| Original language | English |
|---|---|
| Pages (from-to) | 1218-1220 |
| Number of pages | 3 |
| Journal | Key Engineering Materials |
| Volume | 336-338 II |
| DOIs | |
| State | Published - 2007 |