Abstract
The pitting corrosion behavior of reinforcing steel in cement mortar has been studied by electrochemical noise analysis (ENA) method. The wavelet Sym4 has been applied to analyze the EN data of reinforcing steel in mortar. The energy distribution plot(EDP) was plotted. The experimental results demonstrated that the change of EDP during the corrosion process could qualitatively reveal the useful information of corrosion mechanism. According to EDP, the occurance of pitting corrosion can be identified qualitativly.
| Original language | English |
|---|---|
| Pages (from-to) | 365-369 |
| Number of pages | 5 |
| Journal | Corrosion Science and Protection Technology |
| Volume | 21 |
| Issue number | 4 |
| State | Published - 2009 |
| Externally published | Yes |
Keywords
- Corrosion monitoring
- Electrochemical noise
- Pitting corrosion
- Wavelet analysis
Fingerprint
Dive into the research topics of 'Pitting corrosion characters of reinforcing steel in cement mortar'. Together they form a unique fingerprint.Cite this
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver