@article{0c1fe4e0f59b48fe9382e311919068e4,
title = "Nanoindentation characterisation of the properties around reinforcements in a heat treated spray deposited 2014+15vol\%SiCp metal-matrix composite",
author = "Zhang, \{J. S.\} and Liu, \{X. J.\} and H. Cui and Sun, \{Z. Q.\} and Chen, \{G. L.\}",
year = "1996",
month = nov,
day = "1",
doi = "10.1016/1359-6462(96)00249-7",
language = "英语",
volume = "35",
pages = "1115--1120",
journal = "Scripta Materialia",
issn = "1359-6462",
publisher = "Acta Materialia Inc",
number = "9",
}