Multiscale simulation and nanoindentation experimental study of initial plasticity of Fe single crystal

  • Harbin Institute of Technology

Research output: Contribution to journalArticlepeer-review

Abstract

It is very important to understand the initial plastic behavior of metals at microscale. In order to research the initial plasticity of body centered cubic metals in micro-/nano-scale, the multiscale simulation method and experimental study were used to study the nanoindentation process of Fe single crystal. The results show that the first abruption of load - displacement curve in nanoindentation of Fe single crystal can be attributed to the first transition from elastic to plastic deformation characterized by the dislocation emission.

Original languageEnglish
Pages (from-to)s458-s462
JournalTransactions of Nonferrous Metals Society of China (English Edition)
Volume19
Issue numberSUPPL. 2
DOIs
StatePublished - Sep 2009

Keywords

  • Dislocation
  • Initial plasticity
  • Multiscale simulation
  • Nanoindentation