The present paper investigated the microstructure and mechanical properties of ZrB2-10 vol.%SiCp-10 vol.%ZrO2 composites hot pressed at three temperatures. Phase transformability from t-ZrO2 to m-ZrO2 during fracture was analyzed through calculating the volume fractions of m-ZrO2 and t-ZrO2 on polished and fracture surfaces. The densification temperature was found to have a significant effect on the microstructure, phase transformation and the properties of the composites. When the composite was hot pressed at 1950 °C, the average grain size was 9.5 μm, and the fracture toughness was 4.5 MPa·m1/2. Comparatively, when the composite was hot pressed at 1750 °C, the average grain size was 3.4 μm, and the fracture toughness increased by ~ 50% to 6.8 MPa·m1/2.
| Original language | English |
|---|---|
| Pages (from-to) | 2404-2406 |
| Number of pages | 3 |
| Journal | Materials Letters |
| Volume | 62 |
| Issue number | 16 |
| DOIs | |
| State | Published - 15 Jun 2008 |
Keywords
- Densification temperature
- Mechanical properties
- Microstructure
- Phase transformation
Fingerprint
Dive into the research topics of 'Microstructure and mechanical properties of hot pressed ZrB2-SiCp-ZrO2 composites'. Together they form a unique fingerprint.Cite this
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver