title = "Mechanical connection between 8YSZ ceramic and 7075 aluminum alloy",
abstract = "The 8YSZ ceramic coating material was prepared by hot-pressing sintering, and the mechanical connection between 8YSZ ceramic coating materials and 7075 aluminum alloy through the mosaic structure was presented as a new connection method. The change rules of mechanical properties such as density test, bending strength and toughness in different sintering process were researched. The results show that density is increased and grains are grown up gradually with the increasing sintering temperature without any microstructure defects. The optimal mechanical properties are obtained by sintering temperature at 1500°C.",
keywords = "8YSZ, Hot-pressing sintering, Mechanical connection, Shear strength, Simulation",
author = "Du, \{Zhi Ming\} and Jin Qin and Sun, \{Yong Gen\} and Niu, \{Jia Hong\} and Zhao, \{Wang Qi\}",
year = "2013",
doi = "10.4028/www.scientific.net/AMR.834-836.315",
language = "英语",
isbn = "9783037859162",
series = "Advanced Materials Research",
pages = "315--319",
booktitle = "Research in Materials and Manufacturing Technologies",
note = "2013 3rd International Conference on Materials and Products Manufacturing Technology, ICMPMT 2013 ; Conference date: 25-09-2013 Through 26-09-2013",
}