Material flow pattern in friction stir welding of AZ31 magnesium alloy

  • Hua Zhang*
  • , Li Jie Guo
  • , San Bao Lin
  • , Lin Wu
  • , Ji Cai Feng
  • *Corresponding author for this work
  • Harbin Institute of Technology

Research output: Contribution to journalArticlepeer-review

Abstract

A thin Cu coating was deposited on both sides of AZ31 magnesium alloy to be joined to study the material flow in friction stir welding. The results show that the probe wipes the material from the advancing side into a rotating and moving zone, and material rotates, advances, and descends helically in the stir zone and rises in the outer part of the rotating zone.

Original languageEnglish
Pages (from-to)67-69
Number of pages3
JournalHanjie Xuebao/Transactions of the China Welding Institution
Volume25
Issue number4
StatePublished - Aug 2004

Keywords

  • AZ31 magnesium alloy
  • Advancing side
  • Friction stir welding
  • Material flow
  • Retreating side