Skip to main navigation Skip to search Skip to main content

Low temperature brittle fracture resistance of asymmetrical synchronous double-sided arc welded joint of 10Ni5CrMoV steel

  • Lu Liu
  • , Jiayou Wang
  • , Dayong Li
  • , Guangjun Zhang*
  • *Corresponding author for this work
  • Jiangsu University of Science and Technology
  • Harbin Institute of Technology

Research output: Contribution to journalArticlepeer-review

Abstract

Low temperature brittle fracture resistance of asymmetrical synchronous double-sided arc welded (DSAW) joint of 10Ni5CrMoV steel was investigated by series temperature impact test, dynamic tear test and drop hammer test. The results show that DSAW joints of steel 10Ni5CrMoV have a practicable brittle fracture resistance. The impact energy value on the fusion line of DSAW joint meets the technical requirement of the 10Ni5CrMoV steel (i.e., Akv(-50℃≥47 J) with a large allowance. Minimum of dynamic tearing energy at -1℃ is 1150 J, higher than the standard of 644 J DT work at 0℃. Drop hammer test determines that the nil-ductility transition temperature of weld metal of 10Ni5CrMoV steel is -80℃, elastic fracture transition temperature is -47℃, full plastic fracture transition temperature is -14℃.

Original languageEnglish
Pages (from-to)109-113
Number of pages5
JournalHanjie Xuebao/Transactions of the China Welding Institution
Volume37
Issue number8
StatePublished - 25 Aug 2016

Keywords

  • 10Ni5CrMoV
  • Double-sided arc welding
  • Low temperature toughness

Fingerprint

Dive into the research topics of 'Low temperature brittle fracture resistance of asymmetrical synchronous double-sided arc welded joint of 10Ni5CrMoV steel'. Together they form a unique fingerprint.

Cite this