Abstract
Alumina borate whisker reinforced aluminium metal matrix composites were liquid bonded in air. The liquid filler metal of a Zn-Al eutectic alloy could get into the clearance between composites couples by the action of ultrasonic capillarity. The bond/composite interface was eroded, so that a rough interface formed and the oxide film could be removed completely under the action of ultrasonic vibration for 3 s. The shear strength of the bond increases with ultrasonic time. A removal model for the oxide film on the composites during ultrasonic aided liquid bonding was established.
| Original language | English |
|---|---|
| Pages (from-to) | 81-84 |
| Number of pages | 4 |
| Journal | Materials Science and Technology (United Kingdom) |
| Volume | 27 |
| Issue number | 1 |
| DOIs | |
| State | Published - Jan 2011 |
Keywords
- AlBO/Al composites
- Liquid bonding
- Oxide film removal
- Ultrasonic
Fingerprint
Dive into the research topics of 'Interfacial structure and formation mechanism in ultrasonically aided liquid bonding of Al18B4O33/Al composites in air'. Together they form a unique fingerprint.Cite this
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver