Abstract
In (5 ± 1)°C, 5% in mass MgSO4 corrosion solution, the visual appearance, strength and composition analysis of cement mortars added with different functional chemical admixtures (shrinkage-reducing agent, hardening accelerator, crystal resistance agent) and limestone powder were researched at different storage times. The results indicated that after corroded for 360 days, the thaumasite crystal appeared in all cement mortars added with different functional chemical admixtures. It showed that the functional chemical admixtures used in this experimentation could not solve TSA problem, but some of them (except crystal resistance agent) could delay TSA development at early period (210 days).
| Original language | English |
|---|---|
| Pages (from-to) | 23-25+109 |
| Journal | Wuhan Ligong Daxue Xuebao/Journal of Wuhan University of Technology |
| Volume | 30 |
| Issue number | 4 |
| State | Published - Apr 2008 |
| Externally published | Yes |
Keywords
- Cement mortar
- Chemical admixture
- Sulfate attack
- Thaumasite
Fingerprint
Dive into the research topics of 'Influence of chemical admixtures on anti-TSA performance of cement mortars'. Together they form a unique fingerprint.Cite this
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver