Abstract
Electroplated Ni interlayer was used in the diffusion bonding of ZrC-SiC composite. The interfacial reaction focused on Ni-SiC reaction system. Corresponding reaction products were identified to be Ni2Si and graphite. An optimal Ni interlayer of 4 μm, which was precisely controlled by adjusting the plating time, was designed to ensure a reliable bonding for full ceramic joints. Shear strength of the electroplating assisted joints reaches 183 MPa and 45 MPa at room temperature and 800 C, respectively, which are 9% and 67% higher than that of the traditional joints bonded with thicker Ni foil.
| Original language | English |
|---|---|
| Pages (from-to) | 7613-7616 |
| Number of pages | 4 |
| Journal | Ceramics International |
| Volume | 40 |
| Issue number | 5 |
| DOIs | |
| State | Published - Jun 2014 |
Keywords
- Ceramic
- Diffusion bonding
- Electroplating
- Microstructure
Fingerprint
Dive into the research topics of 'Electroplating assisted diffusion bonding of ZrC-SiC composite for full ceramic joints'. Together they form a unique fingerprint.Cite this
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver