Effects of minor Si addition on glass formation and thermal stability of Ni free Ti-based bulk metallic glass

  • Shengli Zhu*
  • , Guoqiang Xie
  • , Fengxiang Qin
  • , Xinmin Wang
  • *Corresponding author for this work

Research output: Chapter in Book/Report/Conference proceedingConference contributionpeer-review

Abstract

The effects of small amounts of Si on the glass-forming ability, thermal stability and mechanical property of a TiZrCuPdSn bulk metallic glass were investigated. The addition of Si caused the decrease of glass-forming ability and the enlarging of the supercooled liquid (SCL) region. With 2 at.% Si addition, a significant SCL region of 80 K was obtained, which indicated high thermal stability of the glassy alloy and was in favor of secondary working by viscous flow deformation. With increasing Si content, the plasticity decreased.

Original languageEnglish
Title of host publicationAdvanced Materials Science and Technology
PublisherTrans Tech Publications Ltd
Pages36-39
Number of pages4
ISBN (Print)9783037856604
DOIs
StatePublished - 2013
Externally publishedYes
Event8th International Forum on Advanced Materials Science and Technology, IFAMST 2012 - Fukuoka City, Japan
Duration: 1 Aug 20124 Aug 2012

Publication series

NameMaterials Science Forum
Volume750
ISSN (Print)0255-5476
ISSN (Electronic)1662-9752

Conference

Conference8th International Forum on Advanced Materials Science and Technology, IFAMST 2012
Country/TerritoryJapan
CityFukuoka City
Period1/08/124/08/12

Keywords

  • Biomaterial
  • Bulk metallic glass
  • Glass-forming ability
  • Minor element addition
  • Thermal stability