Abstract
Stress corrosion cracking (SCC) behavior of as-extruded alumina borate whisker (Al18B4O33)w reinforced pure aluminum composite in 3.5%NaCl solution was investigated using double cantilever beam (DCB) method. The effect of whisker orientation on the stress corrosion cracking behavior of the composite after extrusion was examined. The results indicated that the crack propagated easily along the interface between whisker and matrix in the composite. The whisker orientation plays an important role in stress corrosion cracking of the composite after extrusion.
| Original language | English |
|---|---|
| Pages (from-to) | 642-646 |
| Number of pages | 5 |
| Journal | Materials Letters |
| Volume | 56 |
| Issue number | 5 |
| DOIs | |
| State | Published - Nov 2002 |
| Externally published | Yes |
Keywords
- Composite
- Extrusion
- Stress corrosion cracking
- Whisker orientation
Fingerprint
Dive into the research topics of 'Effect of whisker orientation on the stress corrosion cracking behavior of alumina borate whisker reinforced pure Al composite'. Together they form a unique fingerprint.Cite this
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver