Abstract
Lead-free K0.5Na0.5NbO3 thin films with different excess ratios of alkali metal were prepared by chemical solution deposition method. The volatilization rate of the K, Na elements at a certain temperature was calculated by EDS analysis. The volatilization rate of K element is 55% and Na element is 10% when the KNN thin film was pre-sintered at the temperature of 375 °C and then final heated at the temperature of 675 °C. The prepared KNN thin films with the right excess ratios (K-55%, Na-10%) obtained uniform and dense microstructure, and gain well ferroelectric property.
| Original language | English |
|---|---|
| Pages (from-to) | 137-145 |
| Number of pages | 9 |
| Journal | Integrated Ferroelectrics |
| Volume | 213 |
| Issue number | 1 |
| DOIs | |
| State | Published - 2021 |
Keywords
- Excess ratio
- KNN
- alkali metal
- ferroelectric property
- microstructure
Fingerprint
Dive into the research topics of 'Effect of Excess Ratio of Alkali Metal on Microstructure and Ferroelectric Property of K0.5Na0.5NbO3 Thin Film'. Together they form a unique fingerprint.Cite this
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver