Abstract

The dry sliding wear properties of Ti-6Al-4V alloy is sliding against GCr15 steel under different velocities (between 0.2 and 1.2 m/s) and applied loads (from 30-90 N) were tested using a pin-on-disk tester in air. The wear occurred on both surfaces of the tested couplings. The wear rate of the Ti-61Al-4V alloy ranged from 23.0 to 123.8 mg/km. The wear of Ti-6Al-4V samples was in severe wear. The wear rate of Ti-6Al-4V samples increased with the increasing load and shows a minimum on the curves of wear rate versus sliding velocity. SEM morphologies of worn surfaces and debris were observed. Phases in the debris were analyzed by means of XRD spectra.

Original languageEnglish
Pages (from-to)67-71
Number of pages5
JournalJournal of Harbin Institute of Technology (New Series)
Volume9
Issue number1
StatePublished - Mar 2002

Keywords

  • Delamination
  • Dry sliding
  • Oxidization
  • Titanium alloy
  • Wear

Fingerprint

Dive into the research topics of 'Dry sliding wear behavior of Ti-6Al-4V alloy in air'. Together they form a unique fingerprint.

Cite this