Abstract
In the original article, there is an error in Figure 1. The unit of Specific strength should be MPa/(g•cm-3).
| Original language | English |
|---|---|
| Pages (from-to) | 1437 |
| Number of pages | 1 |
| Journal | Metallurgical and Materials Transactions A: Physical Metallurgy and Materials Science |
| Volume | 51 |
| Issue number | 3 |
| DOIs |
|
| State | Published - 1 Mar 2020 |
| Externally published | Yes |
Fingerprint
Dive into the research topics of 'Correction to: Network-Strengthened Ti-6Al-4V/(TiC+TiB) Composites: Powder Metallurgy Processing and Enhanced Tensile Properties at Elevated Temperatures (Metallurgical and Materials Transactions A, (2019), 50, 8, (3629-3645), 10.1007/s11661-019-05244-7)'. Together they form a unique fingerprint.Cite this