Abstract
In this study, fluoridated hydroxyapatite coatings are prepared on Ti6Al4V alloy substrate through sol-gel method. The bonding strength is evaluated through two different methods: pull-out method and scanning scratch method. Both results show F incorporation could effectively increase the bonding between coating and substrate. It is found that the pull-out results are actually compounds of adhesion failure, cohesive failure and glue failure; while the critical loads in scanning scratch show only the coating-matrix adhesion strength. It is suggested that scanning scratch test is more suitable to evaluate the bonding strength of bioactive ceramic coatings.
| Original language | English |
|---|---|
| Pages (from-to) | 5361-5364 |
| Number of pages | 4 |
| Journal | Thin Solid Films |
| Volume | 517 |
| Issue number | 17 |
| DOIs | |
| State | Published - 1 Jul 2009 |
| Externally published | Yes |
Keywords
- Bonding strength
- Coating
- Failure mode
- Fluoridated hydroxyapatite
Fingerprint
Dive into the research topics of 'Bonding strength of fluoridated hydroxyapatite coatings: A comparative study on pull-out and scratch analysis'. Together they form a unique fingerprint.Cite this
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver