Pure zinc foil was selected as an interlayer to improve the strength of the AZ31B Mg/7075-T6 Al dissimilar alloys friction stir lap welding joint. Compared with the conventional lap joint, the joint with the zinc interlayer has a higher effective sheet thickness, a larger effective lap width and a wider stir zone. The dispersed Mg-Zn intermetallic compounds are achieved instead of the continuous Mg-Al intermetallic compounds, improving the tensile shear load. The maximum fracture load of the joint with the zinc interlayer reaches 6.6 K N at the rotating velocity of 1000 rpm.
| Original language | English |
|---|---|
| Pages (from-to) | 82-90 |
| Number of pages | 9 |
| Journal | Journal of Materials Processing Technology |
| Volume | 263 |
| DOIs | |
| State | Published - Jan 2019 |
| Externally published | Yes |
Keywords
- AZ31B Mg/7075-T6 Al
- Friction stir lap welding
- Mechanical properties
- Microstructures
- Zinc interlayer
Fingerprint
Dive into the research topics of 'AZ31B/7075-T6 alloys friction stir lap welding with a zinc interlayer'. Together they form a unique fingerprint.Cite this
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver