Abstract
Alumina ceramic coating of aluminum alloy surface was performed using micro-plasma oxidation (MPO) technology. Coating formed after short treatment time was found to consist of α-Al2O3 and γ- Al2O3. Single α-Al2O3 coatings can be gained by oxidation for 2.5 h. The growth velocity of coating thickness was 0.7 μm/min during first 135 min, then that was constant. The surface density of coating was only 0.088 mg/cm2 at 15th min, then that increases gradually. The surface density increase presented a linear relationship during 15-60 min, and after 60 min the increase of surface density of coating is slow.
| Original language | English |
|---|---|
| Pages (from-to) | 651-654 |
| Number of pages | 4 |
| Journal | Xiyou Jinshu Cailiao Yu Gongcheng/Rare Metal Materials and Engineering |
| Volume | 33 |
| Issue number | 6 |
| State | Published - Jun 2004 |
Keywords
- Aluminum alloy
- Ceramic coatings
- Micro-plasma oxidation
Fingerprint
Dive into the research topics of 'Analysis of growth characteristic of alumina coatings by micro-plasma oxidation'. Together they form a unique fingerprint.Cite this
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver