Abstract

To investigate the mechanical properties of alkali-activated slag ceramsite concrete blocks after exposure to high temperature, compression tests were conducted on 48 alkali-activated slag ceramsite concrete blocks with two strength grades, MU10 and MU20, and all the specimens were exposed to normal temperature and a temperature history of 400℃, 600℃, 700℃, 800 ℃, 900℃, 1 000℃, and 1 100℃. The results show that the compressive strengths of MU10 and MU20 ceramsite concrete blocks exhibited a linear decrease with the increase of the heating temperature from 20℃ to 1 100℃. Based on the test results, the formulas were constructed to calculate the compressive strengths of the alkali-activated slag ceramsite concrete blocks after exposure to high temperature in term of the heating temperatures.

Translated title of the contributionMechanical properties of alkali-activated slag ceramsite concrete block after exposure to high temperature
Original languageChinese (Traditional)
Pages (from-to)46-50
Number of pages5
JournalHarbin Gongye Daxue Xuebao/Journal of Harbin Institute of Technology
Volume51
Issue number6
DOIs
StatePublished - 30 Jun 2019

Fingerprint

Dive into the research topics of 'Mechanical properties of alkali-activated slag ceramsite concrete block after exposure to high temperature'. Together they form a unique fingerprint.

Cite this